Product Description:

PA TW341 is a heat Stabilized, wear and friction modified PA46.

Applications:

Advanced engineering application such as auto parts.

Typical data:

PROPERTY TEST METHOD UNIT TYPICAL VALUE
Molding shrinkage (parallel) ISO 294-4 % `2 / *
Molding shrinkage (normal) ISO 294-4 % 2 / *
Tensile modulus ISO 527-1/-2 MPa 3300
Tensile modulus (120°C) ISO 527-1/-2 MPa 800
Tensile modulus (160°C) ISO 527-1/-2 MPa 650
Tensile modulus (180°C) ISO 527-1/-2 MPa 600
Tensile modulus (200°C) ISO 527-1/-2 MPa 500
Yield stress ISO 527-1/-2 MPa 100 / 55
Yield stress(120°C) ISO 527-1/-2 MPa 50
Yield stress(160°C) ISO 527-1/-2 MPa 40
Yield stress(180°C) ISO 527-1/-2 MPa 35
Yield stress(200°C) ISO 527-1/-2 MPa 30
Nominal strain at break ISO 527-1/-2 % 40/ >50
Nominal strain at break(120°C) ISO 527-1/-2 % >50
Nominal strain at break(160°C) ISO 527-1/-2 % >50
Nominal strain at break(180°C) ISO 527-1/-2 % >50
Nominal strain at break(200°C) ISO 527-1/-2 % >50
Flexural modulus ISO 178 MPa 3000 / 900
Flexural modulus(120°C) ISO 178 MPa 800
Flexural modulus(160°C) ISO 178 MPa 600
Charpy impact strength (+23°C) ISO 179/1eU kJ/m2 N/N
Charpy impact strength (-30°C) ISO 179/1eU kJ/m2 N/N
Charpy notched impact strength (+23°C) ISO 179/1eA kJ/m2 10/ 35
Charpy notched impact strength (-30°C) ISO 179/1eA kJ/m2 4/4
Izod notched impact strength (+23°C) ISO 180/1A kJ/m2 10/35
Izod notched impact strength (-40°C) ISO 180/1A kJ/m2 4/4
Melting temperature (10°C/min) ISO 11357-1/-3 °C 295 / *
Temp. of deflection under load (1.80 MPa) ISO 75-1/-2 °C 190 / *
Temp. of deflection under load (0.45 MPa) ISO 75-1/-2 °C 280/*
Coeff. of linear therm. expansion (parallel) ISO 11359-1/-2 E-4/°C 0.85/ *
Coeff. of linear therm. expansion (normal) ISO 11359-1/-2 E-4/°C 1.1 / *
Burning Behav. at 1.5 mm nom. thickn. IEC 60695-11-10 class V-2 / *
Thickness tested IEC 60695-11-10 mm 1.5 / *
UL recognition - - Yes / *
Burning Behav. at thickness h IEC 60695-11-10 class V-2 / *
Thickness tested IEC 60695-11-10 mm 0.75 / *
UL recognition - - Yes / *
Relative Temperature Index – electrical UL746B °C 150
RTI electrical(Thickness (1) tested) UL746B mm 0.75
Thermal Index 5000 hrs IEC 60216/ISO 527-1/-2 °C 152
Volume resistivity IEC 60093 Ohm*m 1E13 / 1E7
Electric strength IEC 60243-1 kV/mm 25/15
Comparative tracking index IEC 60112 - 400 /-
Relative permittivity (1Hz) IEC 60250 - 3.6/4.5
Humidity absorption Sim. to ISO 62 % 3.7/ *
Density ISO 1183 kg/m3 1180 / -

* Typical values not to be construed as specifications.